Description
Black Plastic-Vinyl Chloride/Acetate Copolymer
Smooth Matte Surface – Plasticizer Free
Used in ASTM D 2486, ASTM D 4213, ISO 11998 and Other Scrub Test Methods
In a typical scrub test, the coating is applied to the Leneta Scrub Test Panel at a specified film thickness, allowed to dry, then subjected to scrubbing with a straight-line scrub tester. In ASTM D 2486, a 10 mil shim is inserted under the panel to accelerate failure and thereby reduce testing time. The scrub resistance is the number of scrub cycles required to remove the coating to a specified end point. Alternatively, the loss in weight is determined after a specified number of scrub cycles as a measure of scrub resistance, with calculation of equivalent loss in film thickness.
Leneta Scrub Test Panels have a special, finely textured surface for enhanced adhesion. As paints are gradually worn down during the scrubbing process, a feathered edge” is produced which allows for a more precise determination of the end point
Features
- Plastic-Vinyl Chloride/Acetate Copolymer
- Smooth Matte Surface
- Plasticizer Free
- Used in ASTM D 2486, ASTM D 4213, ISO 11998 and Other Scrub Test Methods
- Have a special, finely textured surface for enhanced adhesion.
Technical Attributes
| Size: | 6-1/2 x 17 in (165 x 432 mm) |
| Thickness: | 10 mil (0.25 mm) |
| Quantity Per Box: | 100 |
| Boxes per Case: | 5 |
Standards
ASTM D2486, ASTM D3450, ASTM D4213, ASTM D4828, ASTM D6900, ASTM D7190, ASTM D7377, ISO 11998
Procedure
In a typical scrub test, the coating is applied to the Leneta Scrub Test Panel at a specified film thickness, allowed to dry, then subjected to scrubbing with a straight-line scrub tester. In ASTM D 2486, a 10 mil shim is inserted under the panel to accelerate failure and thereby reduce testing time. The scrub resistance is the number of scrub cycles required to remove the coating to a specified end point.
Alternatively, the loss in weight is determined after a specified number of scrub cycles as a measure of scrub resistance, with calculation of equivalent loss in film thickness.
As paints are gradually worn down during the scrubbing process, a feathered edge” is produced which allows for a more precise determination of the end point.